Hello Joe,
Try soaking the whole lower assembly in a mixture of diesel and paraffin (50:50) for at least a week. Then apply heat to just the aluminium casting.
There is also a very good release fluid in a spray can 'Bulldog BDX' that I have found to be very effective at freeing seized parts.
Link:
Bulldog_BDX
As for the heat, have you tried an induction heater as used by plumbers/engineers to heat localised areas of metal rather than heating the whole assembly. Also for rapid cooling of an area an aerosol can of water pipe freezing fluid can help quickly contract metal.
I hope this helps.
Good health, Bill
Hallo Joe,
Versuchen Sie, die gesamte untere Baugruppe mindestens eine Woche lang in einer Mischung aus Diesel und Paraffin (50:50) einzuweichen. Dann Wärme nur auf das Aluminiumgussteil anwenden.
Es gibt auch eine sehr gute Trennflüssigkeit in einer Spraydose 'Bulldog BDX', die meiner Meinung nach sehr effektiv bei der Befreiung festgefressener Teile ist.
Link:
Bulldog_BDX
Was die Hitze betrifft, haben Sie eine Induktionsheizung ausprobiert, wie sie von Klempnern / Ingenieuren verwendet wird, um lokalisierte Metallbereiche zu erhitzen, anstatt die gesamte Baugruppe zu erhitzen. Auch zum schnellen Kühlen eines Bereichs kann eine Aerosoldose mit Gefrierflüssigkeit für Wasserleitungen helfen, Metall schnell zusammenzuziehen.
Ich hoffe das hilft.
Gute Gesundheit, Bill